Advice 1: Than to patch the crack on the shell

Despite the fact that the shell outwardly – the subject is quite strong, she still may be subject to certain deformations. For example, most of the shell cracking. And then, before the landlord raises the question: how did this crack to close up? And can it be done at all or would have to completely change the sink?
Than to patch the crack on the shell
Crack on the shell may be a huge number of reasons. For example, you dropped something. Or often pour hot water. In any case, whatever caused the crack, it is worth remembering that not necessarily immediately put on the shell cross. In some cases it is quite possible to save.

How to fix a crack in the sink



You need to pay attention to the material from which made the shell. Indeed, for each specific substance has its own repair methods.

For example, you have a metal shell and covered with enamel. In this case, do not worry – it will last you a very long time. Crack this shell is formed exclusively in the enamel. Enamel can be corrected in different ways.

The first is to make a overlay, for example, acrylic. The principle of recovery of the shell is the same as the bath. Simply made to order in sizes suitable insert, which is placed later in the sink and secured at the edges. As a result you get a new sink that will delight with its pure white and has no defects.
Do not think that if the sink itself was not damaged, it can not be repaired. Remember – water, falling on a defect in the form of scratches, aggravates it: there is a rust, black mold, etc.


The second option is to use a sealant. There are many modern tools that are intended to furnish items under prolonged influence of water. Enough to give you the best and repair the scratch. The principle of repair is quite simple: dry the sink, slide degreasing the edges of the crack, then wipe everything with a dry cloth and promazhte sealant.

If cracked ceramic or porcelain sink will fit the same way as with metal, the use of sealant. The scheme of using the same.
Despite the fact that a ceramic shell can be glued, all the experts recommend not to delay and to change it as soon as possible to avoid unpleasant surprises.


Popular today of sinks made of artificial stone, despite its strength and reliability can also suffer from substandard care and crack. In this case, you will epoxy glue or a similar adhesive. Gently RUB them damage, and it will no longer be evident.

In very advanced cases, it is necessary to resort to more drastic repair – drilling and deep-sealing damaged surfaces.

What you should consider



So you don't have to wonder what to do, try to think in advance about prevention. Do not pour boiling water in a sink, for example, drain the water from the just boiled potatoes. And, of course, do not include the followed by cold. Such temperature changes even a strong material will not stand.

Of course, be careful when holding heavy jars, pans or pots. Don't drop them, or crack you with almost 100% probability provided.

People often refer to the shells as minor complements the subject in the house. But if you give her some attention and try to treat it gently, it will serve you for a long time and no repairs will be required.

Advice 2 : How to fix skol

From chips, no one is immune. Even on the new bathroom you may receive such an undesirable element. Of course, no desire to change the bath to put a liner or to emulirovat one single chip. What should I do? To remove the chip, of course. Of course, you need to understand that perfectly match the shades in halftones is obtained infrequently, so even the naked eye will be visible where it was chipped. Still, it's better than leaving things as they are.
The chip or crack is no reason to change the bath
You will need
  • Autosplice any. You should take a tube of small size and bright colors it is better to certainly not color their way through the enamel;
  • A fine-grained emery paper;
  • Enamel bath;
  • Abrasive polishing paste;
  • Tinting paste (if you do not have a white tub);
  • Construction (can be regular), the Hairdryer;
  • Solvent for degreasing the surface of the bath;
  • Polishing paste and felt.
Instruction
1
Clean the crack or chip to the steel color, then dry with a Hairdryer, then degrease the cleaned area with some solvent or acetone.
2
Prepare the putty, apply it to the chip and allow to dry for about 15-30 minutes. The drying time of filler depends on its grade. After drying putty sand it with sandpaper until the disappearance of the slightest bumps. Even better would be to smooth out the putty with a little pressure so that it is up to the level of the bath is not reached quite a bit. Then still enough space for the enamel. Then again, degrease and dry the surface with a Hairdryer.
3
Next is preparing the enamel. Take one part of hardener and four parts of the framework. If needed, add in the color. Kohler much to add not be (enough for 5-7%). Cover the prepared enamel place of cleavage. Allow the enamel to dry.
4
As soon as the enamel has dried, RUB the spot fine sandpaper. Then Polish with polishing paste and felt. So you get rid of traces of "grain" emery paper and finally will align the place of cleavage. That's all.